Welding rod for
TIG-Welding Process |
|
|
|
|
Standards: |
EN 12072
|
W 19 9 L
|
|
DIN 8556
|
SG X2 Cr Ni
19 9 |
|
AWS/ASME SFA
5.9 |
ER 308 L
|
|
TS 11197
|
SG X2 Cr Ni
19 9 |
|
M.No:
|
1.4316
| |
|
Application and Properties: |
Austenitic stainless
steel welding rod for TIG-welding of unstabilized or
stabilized corrosion resisting Cr-Ni steels. Resistant
to intergranular corrosion up to 350˚C. Non-scaling up
to 800˚C, in air or oxidizing combustion gases.
|
|
Materials:
|
1.4301 |
X 4 Cr Ni 18 - 10
|
X 4 Cr Ni 18 - 10
|
304, 304H |
1.4303 |
X 4 Cr Ni 18 - 12
|
X 4 Cr Ni 18 - 12
|
305, 308 |
1.4306 |
X 2 Cr Ni 19 - 11
|
X 2 Cr Ni 19 - 11
|
304L |
1.4311 |
X 2 Cr Ni N 18 -
10 |
X 2 Cr Ni N 18 -
10 |
304LN |
1.4541 |
X 6 Cr Ni Ti 18 -
10 |
X 6 Cr Ni Ti 18 -
10 |
321 |
1.4550 |
X 6 Cr Ni Nb 18 -
10 |
X 6 Cr Ni Nb 18 -
10 |
347 |
1.4552 |
GX 5 Cr Ni Nb 19 -
10 |
GX 5 Cr Ni Nb 19 -
10 |
- |
1.4300 |
X 12 Cr Ni 18 - 8
|
X 12 Cr Ni 18 - 8
|
302 |
|
Please observe
admissible operating temperatures for welding consumable
and base metal |
|
Analysis
of Wire Electrode/Rod (typical values in %) : |
<
0.03 |
1.00-2.50 |
0.30-0.65 |
19.5-22.0 |
9.0-11.0
|
|
|
Mechanical
Properties of All-Weld Metal (single values are typical
values): |
|
AW : As welded |
|
Chemical
compositions and mechanical properties apply to
the use shielding gas |
|
: EN
439 - I1 (100% Argon) | |
|
Shielding gas
as to EN 439 |
: I1 (100% Argon)
| |
|
Wire electrode
for MIG/MAG welding |
: INERTFIL 308
LSi | |
Shielding gas
consumption |
: approx. 10
l/min | |
|
Packing
& Order Information : |
2221005 |
1.20 |
1000 |
6 |
2221008 |
1.60 |
1000 |
6 |
2221009 |
2.00 |
1000 |
6 |
2221010 |
2.40 |
1000 |
6 |
2221012 |
3.20 |
1000 |
6 |
|
|
Type of
Current/Polarity/Welding Positions : |
You can click on
the figure to see its explanation... |
|
|