Wire electrode for
Submerged-Arc Welding |
|
|
|
|
Standards: |
EN 756 |
S 2
|
|
DIN 8557
|
S 2
|
|
AWS/ASME
SFA-5.17 |
EM 12 K
|
|
TS 5387
|
S 2
| |
|
Application and Properties: |
Solid, submerged arc
welding wire suitable for welding general structural
steels with medium and high tensile strength, used in
pressure vessel, boiler, pipe, shipbuilding and steel
constructions. Copper coating increases electrical
conductivity and resistance against rusting. |
|
|
|
Qualification
Tests |
: TSE
| |
|
All-Weld
Metal Analysis (typical values in %) : |
FRO AS 231 |
0.025-0.05 |
1.1-1.5
|
0.5-1.1
|
<0.02
|
0.03
|
FRO AS 461 |
0.03-0.05 |
1.0-1.6
|
0.2-0.6
|
<0.02
|
<0.025 |
OP 176 |
0.05 |
1.5 |
0.7 |
0.008
|
0.018
|
OP 139 |
0.062
|
1.30 |
0.2 |
0.009
|
0.019
|
|
|
Analysis
of Wire Electrode/Rod (typical values in %) : |
|
|
Mechanical
Properties of All-Weld Metal (single values are typical
values): |
FRO
AS 231 |
AW /
KS |
>400 |
520-650 |
>22 |
>50 |
>27 |
|
|
|
FRO
AS 461 |
AW /
KS |
>420 |
510-650 |
>22 |
|
>100 |
>50 |
>27 |
|
OP
176 |
AW /
KS |
410
|
530
|
28
|
100 |
65 |
60 |
40 |
|
OP
139 |
AW /
KS |
420
|
520
|
28
|
|
200 |
|
170 |
70 |
|
AW : As welded |
|
Packing
& Order Information : |
2032008 |
1.60 |
25 |
2032009 |
2.00 |
25 |
2032010 |
2.40 |
25 |
2032012 |
3.20 |
25 |
2032013 |
4.00 |
25 |
2032014 |
5.00 |
25 |
2032108 |
1.60 |
250 |
2032109 |
2.00 |
250 |
2032110 |
2.40 |
250 |
2032112 |
3.20 |
250 |
2032113 |
4.00 |
250 |
2032114 |
5.00 |
250 |
|
|
Type of
Current/Polarity/Welding Positions : |
You can click on
the figure to see its explanation... |
|
|