Covered electrode for Welding Stainless and Heat
Resisting Steels
|
Rutile Covering |
|
|
|
Standards: |
EN 1600 |
E 23 12 2 LR
53 |
|
DIN 8556
|
E 23 13 2
MPR 36 160 |
|
AWS/ASME
SFA-5.4 |
E 309Mo - 16
|
|
TS 2716
|
E 23 13 2
MPR 160 36 |
|
TS 2716 EN
1600 |
E 23 12 2 LR
53 | |
|
Application and Properties: |
High-efficiency electrode
for welding dissimilar steels (ferritic to austenitic
steels and depositing austenitic stainless claddings.
Weld metal recovery of 160 %. The austenitic weld metal
has a delta-ferrite content of approx. 15 %. Claddings
on unalloyed steels are already corrosion resistant in
the first layer. Highest operating temperature for
dissimilar steel joints is + 300°C. Possible to use
equally well both with AC and DC. Easy arc striking and
restriking. Fine metal droplet transfer, good fusion of
joint faces, finely rippled bead surface, easy slag
removal. |
|
|
|
Qualification Tests |
: TSE
| |
|
All-Weld Metal Analysis (typical
values in %) : |
|
|
Mechanical Properties of
All-Weld Metal (single values are typical values): |
|
|
|
Redrying: Generally
not required. We recommend redrying 2 hrs. at 300 C |
|
Welding Current [A]: |
55-80 |
70-110 |
110-165 |
150-225 |
|
|
Packing & Order Information
: |
1092004 |
2.00 |
300 |
75 |
1.30 |
1092010 |
2.50 |
350 |
60 |
1.80 |
1092016 |
3.20 |
350 |
40 |
2.00 |
1092020 |
4.00 |
350 |
25 |
1.80 |
1092028 |
5.00 |
350 |
15 |
1.70 |
|
|
Type of Current/Polarity/Welding Positions
: |
You can click on
the figure to see its explanation... |
|
|